Image de la structure interne FDM

SLS et MJF

It is recommended that any sections which are greater in thickness than 7mm for SLS or 10mm for MJF have hollow sections in order to maintain part geometry and minimise warping. Sections greater than 7mm and 10mm are susceptible to warping due to the concentrated energy (heat) located in the part during printing.

In some cases orientating the part at an angle inside the printer can negate warping, as the reduced cross-sectional area minimises the amount of energy used in the layering process. Where it is recommended to hollow a part it may also be preferable to remove all support material too, therefore a drain hole will be added as well (see Support Material)

Ricoh 3D analysera les pièces présentant de grandes zones supérieures à 7 mm et les orientera ou les creusera afin de réduire les risques de déformation lors de l’impression. Cette étape sera effectuée par nos ingénieurs avant l’impression et n’est pas prise en compte lors de la conception.

La prise en compte des trous de drainage et des sections creuses plus épaisses sera effectuée par nos ingénieurs avant l’impression, et nous demanderons toujours votre approbation au préalable.

Tous les fichiers envoyés à Ricoh 3D sont analysés avant l’impression. Nous vous informerons de tout problème de géométrie susceptible d’entraîner des difficultés lors de l’impression ou du post-traitement.

Sections creuses

Besoin d’aide ?

Que vous recherchiez un conseil à propos de matériels, d’un devis ou si vous voulez tout simplement en savoir plus sur la fabrication additive, nous serons ravis de vous aider.
  • Nous appeler

    +44 (0) 800 304 7196

  • Nous contacter

    Nous contacter

    nous envoyer une demande